The key steps in the production process of automotive aluminum sheet are as follows:
Melting and Casting
Precise Composition Control: Strictly control the ratio of alloying elements, such as aluminum, magnesium, silicon, and copper, to ensure they are within specified ranges to meet the diverse performance requirements of automotive sheet. For example, the ratio of magnesium to silicon in 6-series aluminum alloys requires precise control to achieve the appropriate strengthening phase.
Purity Guarantee: Advanced refining technology is used to minimize gas content. For example, hydrogen content must be kept to an extremely low level. The number and size of inclusions can also be reduced. This can be achieved through online degassing and filtration.
Ingot Quality Control: The ingot surface should be smooth and free of obvious defects, and the internal structure should be uniform, free of shrinkage cavities or porosity. Parameters such as casting temperature, speed, and cooling conditions must be properly controlled.
Hot Rolling
Temperature Control: The heating temperature is generally between 450°C and 550°C, ensuring uniform heating of the ingot. The final rolling temperature is typically controlled between 300°C and 350°C to ensure the sheet's microstructure and properties.
Adjusting the Reduction and Rolling Speed: The reduction can be higher during the roughing stage and gradually decrease during the finishing stage. The total reduction should be appropriately determined based on product specifications. The rolling speed should be adjusted according to the different stages to ensure both production efficiency and avoid quality issues.
Surface Quality and Dimensional Accuracy Control: Descaling is performed using methods such as high-pressure water descaling to ensure a smooth plate surface. Thickness accuracy must be controlled within a certain range, such as ±0.1mm, and width accuracy also has corresponding requirements.
Cold Rolling
Pickling: Pickling should thoroughly remove scale and impurities from the surface of the hot-rolled plate while avoiding over-pickling, which may cause surface roughness or compromise dimensional accuracy. The pickling solution concentration, temperature, and time should be appropriately adjusted.
Reduction and Shape Control: The appropriate reduction is determined based on the target thickness, generally between 50% and 80%. Advanced shape control systems ensure that the plate flatness meets requirements, such as not exceeding a certain unit per meter.
Thickness Accuracy Control: To maintain thickness tolerances within a narrow range, such as ±0.05mm, precise adjustment of rolling mill parameters such as rolling force and rolling speed is required.
Heat Treatment
Precise Process Parameter Setting: Parameters such as solution treatment temperature and time, as well as aging treatment temperature and time, must be precisely set based on alloy composition and performance requirements to achieve the desired strengthening effect and overall performance.
Uniformity: Ensure uniform heating of the sheet during heat treatment. This can be achieved by optimizing heating equipment and process layout to avoid inconsistent properties caused by localized overheating or undercooling.
Finishing
Surface Treatment: Through mechanical polishing, chemical treatment, and other methods, the sheet surface roughness is maintained to meet specified requirements, such as an Ra value between 0.8 and 1.6μm, with no defects such as scratches or oil stains.
Shape Correction: Stretching and other methods are used to improve sheet shape and ensure flatness meets automotive sheet standards.
Dimensional accuracy review: Accurately measure and adjust the final dimensions of the plate to ensure that dimensions such as length, width, and thickness meet tolerance requirements.